发明名称 |
METHOD FOR PASSIVATING A NICKEL-ALLOY ELEMENT, ELEMENT OBTAINED BY SAID METHOD, AND METHOD FOR MANUFACTURING AN ASSOCIATED PRIMARY CIRCUIT OF A NUCLEAR REACTOR |
摘要 |
The invention relates to a method (120) for passivating an element made of a nickel alloy, which is intended for limiting the corrosion and the cation release of said element in contact with a liquid. The method comprises a step of applying a thermal treatment (126) to at least one surface of the element, the thermal treatment (126) being carried out at a temperature of 500°C to 900°C, in an inert atmosphere made up of at least 99.9% of an inert gas or a mixture of inert gases. The inert atmosphere is at a pressure substantially equal to atmospheric pressure, and the thermal treatment (126) is carried out during a time ranging from ten to fifty hours. |
申请公布号 |
WO2016097374(A1) |
申请公布日期 |
2016.06.23 |
申请号 |
WO2015EP80665 |
申请日期 |
2015.12.18 |
申请人 |
AREVA;COMMISSARIAT À L'ÉNERGIE ATOMIQUE ET AUX ÉNERGIESALTERNATIVES |
发明人 |
BRUSSIEUX, CHARLES;FOUCAULT, MARC;ENGLER, NATHALIE;PERRIN, STÉPHANE;MARCHETTI, LOIC;MOEGLEN, MAGALI;WOUTERS, YVES |
分类号 |
C23C8/10 |
主分类号 |
C23C8/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|