发明名称 |
NONAQUEOUS-ELECTROLYTE SECONDARY-BATTERY NEGATIVE ELECTRODE |
摘要 |
A negative electrode for nonaqueous electrolyte secondary batteries which suppresses generation of gas and increases power characteristics, including a negative electrode current collector and a negative electrode mixture layer placed on the negative electrode current collector. The negative electrode mixture layer is a mixture of a negative electrode active material, a binding agent, and a conductive agent. The negative electrode active material contains silicon. The binding agent includes a binding agent A made of a rubber polymeric compound. A through-thickness cross section of the negative electrode mixture layer halved into a current collector-side region and a surface-side region, has the amount of the binding agent A in the current collector-side region larger than the amount of the binding agent A in the surface-side region and the amount of the conductive agent in the surface-side region is larger than the amount of the conductive agent in the current collector-side region. |
申请公布号 |
US2016351892(A1) |
申请公布日期 |
2016.12.01 |
申请号 |
US201515113911 |
申请日期 |
2015.01.20 |
申请人 |
SANYO ELECTRIC CO., LTD. |
发明人 |
Sugimori Masanori;Yanagida Katsunori |
分类号 |
H01M4/36;H01M4/48;H01M4/62 |
主分类号 |
H01M4/36 |
代理机构 |
|
代理人 |
|
主权项 |
1. A negative electrode for nonaqueous electrolyte secondary batteries, comprising a negative electrode current collector and a negative electrode mixture layer placed on the negative electrode current collector,
wherein the negative electrode mixture layer is a layer of a mixture of a negative electrode active material, a binding agent, and a conductive agent; the negative electrode active material contains silicon; the binding agent includes a binding agent A made of a rubber polymeric compound; and in the case where a through-thickness cross section of the negative electrode mixture layer is halved into a current collector-side region and a surface-side region, the amount of the binding agent A in the current collector-side region and the amount of the conductive agent in the surface-side region are larger than the amount of the binding agent A in the surface-side region and the amount of the conductive agent in the current collector-side region, respectively. |
地址 |
Daito-shi JP |