摘要 |
<P>PROBLEM TO BE SOLVED: To provide a plastic grout material usable for all portions, particularly for a rear surface cavity of a lining concrete with thin lining, and easily controlling an introduced air quantity. <P>SOLUTION: To manufacture a plastic grout material according to the method of manufacturing by this invention, a hydraulic kneaded material is firstly manufactured by kneading water, sand, and cement (101). Besides, a thickener slurry is manufactured according to the following procedure. A foaming agent-added solution is manufactured by adding the foaming agent to the water and stirring and mixing the mixture (102). A foaming agent such as an alkyl sulfate surface active agent can be used. Next, a bentonite as an inorganic thickener is added to the foaming agent-added solution generated by the stirring and mixing, and the mixture is stirred and mixed to manufacture the thickener slurry (103). Then, the plastic grout material is manufactured by mixing the hydraulic kneaded material with the thickener slurry (104). <P>COPYRIGHT: (C)2009,JPO&INPIT |