发明名称 Roast-leach copper recovery
摘要 A copper-containing sulfidic material is dead-roasted at a temperature of at least 750 DEG C. and the resulting calcine is leached in a sulfuric acid solution to dissolve most of the copper in preference to any iron, nickel and cobalt in the material.
申请公布号 US4168217(A) 申请公布日期 1979.09.18
申请号 US19780894900 申请日期 1978.04.10
申请人 THE INTERNATIONAL NICKEL COMPANY, INC. 发明人 DALVI, ASHOK D.;SRIDHAR, RAMAMRITHAM;BELL, MALCOLM C. E.
分类号 C22B15/00;(IPC1-7):C25C1/12 主分类号 C22B15/00
代理机构 代理人
主权项
地址