PROBLEM TO BE SOLVED: To provide a casting method capable of reducing inclusions captured by a slab in continuous casting for steel.SOLUTION: In continuous casting method blowing an inert gas for steel, equations: 0.07 m≤D≤0.15 m, 0.16 m≤D≤0.3 m, 0.2 m≤L≤0.45 m, (R+R/2)/(D/2)≤4.25(L+L)/D+0.2, (R+R/2)/(D/2)≥0.26(L+L/2)/D+1, 0.3≤(L+L/2)/D≤6.3 and 1.5≤(R+R/2)/(D/2)≤4.0 are satisfied (where, the top edge inside diameter of a nozzle is D; the outside diameter of the nozzle is D; a distance from the top edge of an upper porous refractory to the top edge of a lower porous refractory is L; a distance from the top edge of the lower porous refractory to the lower edge of the lower porous refractory is L; the outside dimension of a nozzle height is L; a distance from the center of the nozzle to the upper porous refractory is R; and the thickness of the upper porous refractory in a radial direction is R).SELECTED DRAWING: Figure 4 |