发明名称 PRODUCTION OF PITCH COKE
摘要 PURPOSE:To obtain a needle coke suitable for use as a starting material for artificial graphite electrodes and having a high quality in a high yield, by treating a raw material comprising a hydrogenated coal tar at a specific temp. in an atmosphere free from oxygen, followed by coking. CONSTITUTION:In producing a pitch coke from a raw material comprising a hydrogenated coal tar, the raw material comprising a hydrogenated coal tar is heat-treated at 340-500 deg.C in an atmosphere free from oxygen, followed by coking. A preferred raw material comprising a coal tar is a tar pitch. Although the tar pitch may be any of a soft pitch having a softening point of 70 deg.C or below, a medium pitch having a softening point of 70-85 deg.C and a hard pitch having a softening point 85 deg.C or above, the soft pitch is preferable from the standpoint of handleability. The degree of hydrogenation is generally in the range of 15-70%, preferably 25-60% in view of the degree of de nitrification.
申请公布号 JPS61293293(A) 申请公布日期 1986.12.24
申请号 JP19850134265 申请日期 1985.06.21
申请人 NIPPON STEEL CHEM CO LTD 发明人 KAJI MASAYOSHI;TORISU TAKESHI
分类号 C10B57/04 主分类号 C10B57/04
代理机构 代理人
主权项
地址