摘要 |
PURPOSE:To obtain a molded article having improved heat resistance readily, by blending a reaction solution for forming a synthetic resin with a specific amount of liquid crystal high polymer powder and subjecting the blend to reaction injection molding. CONSTITUTION:(A) 70-97wt%, preferably 75-95wt% reaction solution for forming a synthetic resin is blended with (B) 3-30wt%, preferably 5-25wt% liquid crystal high polymer which is a rigid straight-chain high polymer to form thermotropic liquid crystal, a rigid straight-chain high polymer to form lyotropic liquid crystal or a rigid side-chain high polymer containing a rigid atom group at the side chain and forming thermotropic or lyotropic liquid crystal and subjected to reaction injection molding.
|