摘要 |
PROBLEM TO BE SOLVED: To provide a manufacturing method for a cobalt-containing oxyhydroxide having large discharge capacity and showing an excellent cycle characteristic without capacity deterioration caused by the progress of charge- discharge cycles when it is used as the positive electrode active material of a battery. SOLUTION: In this manufacturing method for a cobalt-containing oxyhydroxide, a hydroxide expressed by a general formula of Ni1-xCox(OH)2 (0<x<0.5) is processed in an acid solution having pH of 3.5 or above and thereafter oxidized. |