LIGHT-WEIGHT AERATED CONCRETE MIX METHOD USING THE SPECIAL COMPOSITION WITH EMHANCEMENT OF CRACK CONTROL AND FLEXURAL PERFORMANCE |
摘要 |
Disclosed are light-weight aerated concrete composition using admixtures and fibers which are optimally composed to improve a crack control and flexural strength performance during a manufacturing process of light-weight aerated concrete, and a manufacturing method of the light-weight aerated concrete using the same. According to the present invention, the light-weight aerated concrete composition includes: a binding material including 40-80 wt% of cement and 20-60 wt% of admixtures; reinforced fibers having 0.3-1.2 kg per 1 m^3 of the binding material to improve a crack control and flexural strength performance of aerated concrete; 20-40 wt% of water, which serves as mixing water, with respect to the binding material; and 50-70% of foam on a basis of volume after curing the aerated concrete. |
申请公布号 |
KR20160111696(A) |
申请公布日期 |
2016.09.27 |
申请号 |
KR20150036686 |
申请日期 |
2015.03.17 |
申请人 |
KYONGGI UNIVERSITY INDUSTRY & ACADEMIA COOPERATION FOUNDATION |
发明人 |
YANG, KEUN HYEOK;LEE, KYUNG HO |
分类号 |
C04B18/14;C04B16/06;C04B18/08 |
主分类号 |
C04B18/14 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|