发明名称 タイヤ部材及びタイヤの製造方法
摘要 A method for manufacturing a tire member, that improves various performances such as abrasion resistance, tear strength, fatigue resistance and the like of the tire member in good balance is provided. The method includes a step (A) for mixing at least a rubber component, a filler and a thiosulfuric acid compound containing an amino group, and a step (B) for mixing the mixture obtained by the step (A), a sulfur component, and a vulcanization accelerator, wherein the thiosulfuric acid compound containing an amino group is added in an amount of 0.2 parts by mass or more to 100 parts by mass of the rubber component in the step (A), and a temperature of the mixture during mixing is maintained within a range of from 145 to 170° C. for 20 seconds or more in the step (A).
申请公布号 JP6029940(B2) 申请公布日期 2016.11.24
申请号 JP20120245622 申请日期 2012.11.07
申请人 東洋ゴム工業株式会社 发明人 井原 郁夫
分类号 C08J3/20;B60C1/00;C08K3/00;C08K5/41;C08L21/00 主分类号 C08J3/20
代理机构 代理人