发明名称 SECONDARY COOLING METHOD IN CONTINUOUS CASTING
摘要 PROBLEM TO BE SOLVED: To provide a secondary cooling method with which the bulging at the last solidified part is restrained and the center segregation can be prevented when a continuous casting is applied to steel. SOLUTION: Water film flowing is formed at a gap between a water film forming plate continuously shifted in the reverse direction to the drawing-out direction of a cast slab and the cast slab, and the cast slab in the range with which the thickness D of the cast slab and the thickness d of solidified shell satisfy 0.4D<=d<=0.5D, is cooled with the water film flowing.
申请公布号 JP2002086253(A) 申请公布日期 2002.03.26
申请号 JP20000274583 申请日期 2000.09.11
申请人 KAWASAKI STEEL CORP 发明人 ITO YOICHI;TOZAWA KOICHI;TAKEUCHI HIDEJI
分类号 B22D11/124;B22D11/128;B22D11/16;B22D11/22;(IPC1-7):B22D11/124 主分类号 B22D11/124