发明名称 Titanium dioxide methods of production
摘要 The bodies are prepared either by pelleting of a pasty mixture of titanium dioxide powder and titanium dioxide sol and/or 1-20% nitric acid, followed by dehydration and calcination at a temperature of between 400 and 1000° C. for between 0.5 and 3.5 hours; or by preparing pellets from the titanium dioxide powder and added water, annealing of the pellets at between 300 and 500° C., saturation of same with titanium dioxide sol or 1-20% nitric acid in a vacuum, followed by drying and finally annealing at a temperature of between 400 and 1000° C. for between 0.5 and 3 hours.
申请公布号 US6660243(B1) 申请公布日期 2003.12.09
申请号 US20010937156 申请日期 2001.11.20
申请人 SACHTLEBEN CHEMIE GMBH 发明人 PROFT BERND;HIRSCHBERG ELKE;SELING BARBARA;WEYAND SONJA
分类号 B01J20/06;B01J20/28;B01J21/06;B01J35/10;C04B35/46;(IPC1-7):C01G23/047 主分类号 B01J20/06
代理机构 代理人