发明名称 |
COPPER POROUS SINTERED BODY AND COPPER POROUS COMPOSITE MEMBER |
摘要 |
PROBLEM TO BE SOLVED: To provide a copper porous sintered body capable of producing a copper porous sintered body having a small shrinkage ratio at the time of sintering to provide excellent dimensional accuracy and having sufficient strength.SOLUTION: A copper porous sintered body 10 is formed by sintering a plurality of copper fibers 11. The copper fibers 11 are made of copper or a copper alloy, have a diameter R in a range of not less than 0.02 mm and not more than 1.0 mm, and have a ratio L/R of the length L to the diameter R in a range of not less than 4 and not more than 2,500. In a joining part between the copper fibers, oxidation-reduction layers having a porous structure are integrally bonded to each other.SELECTED DRAWING: Figure 3 |
申请公布号 |
JP2016199809(A) |
申请公布日期 |
2016.12.01 |
申请号 |
JP20160150199 |
申请日期 |
2016.07.29 |
申请人 |
MITSUBISHI MATERIALS CORP |
发明人 |
KITA KOICHI;HOSHINO KOJI;SAIWAI TOSHIHIKO;KATO JUN |
分类号 |
B22F3/11;B22F1/00;B22F7/04;C22C1/04;C22C1/08 |
主分类号 |
B22F3/11 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|