摘要 |
A jointed body of heal-resistant alloy, in which surfaces opposed to each other of heat-resistant alloy plates or foils formed on the surfaces thereof with oxide film as necessary are jointed by a composite oxide having a melting point within a temperature range between 800 - 1400 DEG C. Said composite oxide is placed on a portion to be jointed of said heat-resistant alloy plate or foil, subsequently, another heat-resistant alloy plate or foil is placed on said portion to be jointed, and said both heat-resistant alloy plates or foils are heated to a temperature higher than 9/10 of the melting point of said composite oxide, so that said jointed body can be produced. <IMAGE> |
申请人 |
NIPPON STEEL CORP., TOKIO/TOKYO, JP |
发明人 |
KONYA, SHOGO, NIPPON STEEL CORPORATION, SAKAI-SHI, OSAKA 590, JP;OKAMOTO, AKIRA, NIPPON STEEL CORPORATION, SAKAI-SHI, OSAKA 590, JP |