发明名称 Method to eliminate weld solidification cracking of 312 stainless steel overlay and to minimize the overlay's thermal expansion mismatch with carbon steel or low alloy steel substrate
摘要 A method for applying a stainless steel weld overlay on a substrate, e.g., a carbon steel or low alloy steel, uses an arc welding process. The process includes welding a stainless steel weld overlay onto the substrate using a shielding gas mixture including greater than 2% nitrogen by volume with balance being an inert gas or a mixture of inert gases. The nitrogen is of a sufficient concentration so as to eliminate solidification cracking in the weld overlay. In addition, the nitrogen may help to eliminate a mismatch in me coefficient of thermal expansion between the weld overlay and the substrate. Furthermore, if the weld overlay comprises only a single layer, the nitrogen concentration in the shielding gas mixture may be less than 2%.
申请公布号 US6204477(B1) 申请公布日期 2001.03.20
申请号 US19970002119 申请日期 1997.12.31
申请人 WSI WELDING SERVICES, INC. 发明人 LAI GEORGE YING-DEAN
分类号 B23K9/04;B23K35/30;B23K35/38;(IPC1-7):B23K9/00 主分类号 B23K9/04
代理机构 代理人
主权项
地址