发明名称 |
Fremgangsmåte for å forbedre korrosjonsmotstanden for magnesium-aluminium-silisiumlegeringer og magnesiumlegering medforbedret korrosjonsmotstand |
摘要 |
Magnesium alloy with improved corrosion resistance comprising magnesium, 1.5-5 weight % Al, 0.6-1.4 weight % Si, 0.01-0.6 weight % Mn and 0.01-0.4 weight % RE. Method of improving the corrosion resistance of magnesium, aluminium, silicon alloys where Mn is added in order to reduce FE impurities, by keeping both Mn and Fe at a low level by adding small amounts of RE. |
申请公布号 |
NO312106(B1) |
申请公布日期 |
2002.03.18 |
申请号 |
NO19990003289 |
申请日期 |
1999.07.02 |
申请人 |
NORSK HYDRO ASA |
发明人 |
PETTERSEN, KETIL;SKAR, JAN IVAR;VIDEM, MARIANNE |
分类号 |
C22C1/02;C22C23/02;D06C19/00 |