发明名称 Raakakuparin kuumaraffinointi
摘要 Provided herein is a process of fire refining blister copper, comprising the steps of (a) providing molten blister copper into an anode furnace; (b) when sulfur concentration of the molten blister copper provided in step (a) is above a first prescribed target value, oxidizing sulfur in the molten blister copper by blowing oxygen containing gas into the molten blister copper until the first prescribed target value has been reached; (c) subsequently lowering the sulfur and oxygen content in blister copper by blowing inert gas into the molten blister copper until a second prescribed target value has been reached, wherein the inert phase (c) is continued until the second prescribed target value of the oxygen concentration is below 4000 ppm, and the second prescribed target value of the sulfur concentration is below 500 ppm; (d) when sulfur and/or oxygen concentration of the molten blister copper obtained in step (c) is above a third prescribed target value, subsequently reducing oxygen in the blister copper by supplying a reducing agent into the molten blister copper until the third prescribed target value has been reached and anode copper is obtained; and (e) optionally casting the obtained anode copper.
申请公布号 FI20155329(A) 申请公布日期 2016.11.07
申请号 FI20150005329 申请日期 2015.05.06
申请人 Outotec (Finland) Oy 发明人 Jaatinen, Akusti;Talvensaari, Harri
分类号 C22B15/00;C22B5/18;C22B9/05;C22B9/10;C22B15/14 主分类号 C22B15/00
代理机构 代理人
主权项
地址