摘要 |
A composition comprising water atomised prealloyed iron-based steel powder is provided which steel powder comprises by weight-%: 0.2-1.5 Cr, 0.05-0.4 V, 0.09-0.6 Mn, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, the balance being iron. A method of forming a sintered component, and component additionally are provided. |