摘要 |
A method for making a casting nozzle, includes mixing a main casting nozzle material 70-95% by weight and electrofused aggregates 5-30% by weight, the electrofused aggregates consisting essentially of ZrO2 30-60% by weight, Al2O3 20-50% by weight, SiO2 10-20% by weight and SiC 5-40% by weight together with a binder, thereby to make a mixture, forming the mixture in the shape of a casting nozzle thereby to make a formed body, and sintering the formed body. |