摘要 |
<p>The transparent conductive film for an amorphous silicon solar cell is produced by (a) particulating the mixture solution of methanol, pure water, fluorine cpd. and tin compound by the use of an ultrasonic vibrator, and (b) contacting the particulate and a carrier gas to the glass substrate. The glass substrate is pref. silicon oxide (SiO2)-coated soda lime glass, barium borax glass or soda lime glass, the tin cpd. is pref. SnCl2, SnCl2 2H2O, SnCl4, SnCl4 5H2O or (CH3)2SnCl2, the fluorine cpd. is pref. NH4F or HF, and the carrier gas is pref. air, nitrogen or oxygen.</p> |