摘要 |
<p>A process for treating recycled coated broke which has been re-pulped to a slurry for the purpose of recycling the coated broke as cellulose fiber to the paper machine by the addition of a water-soluble polymer dispersion is claimed. The water-soluble polymer is formed by polymerizing a water-soluble mixture which comprises: (a) a cationic monomer represented by the following general formula (I): (see formula) wherein R1 is H or CH3; each of R2, andR3 is an alkyl group having 1 to 2 carbon atoms; R4 is H or an alkyl group of to 2 carbon atoms; A' is an oxygen atom or NH; B' is an alkylene group of 2 to 4 carbon atoms or a hydroxypropylene group; and X' is an anionic counterion; and (b) a second monomer represented by (meth)acrylamide (in an aqueous solution of a polyvalent anionic salt), wherein the polymerization is carried out in the presence of either an organic high-molucular weight multivalent cation comprising a water-soluble polymer containing at least one monomer of formula (1) and/or poly diallyl dimethyl ammonium chloride (DADMAC).</p> |