发明名称 Fe-Ni alloy having high strength and low thermal expansion, a shadow mask made of the alloy, a braun tube with the shadow mask, a lead frame made of the alloy and a semiconductor element with lead frame
摘要 Disclosed is an Fe-Ni alloy consisting of, by mass, 30 to 50% of Ni (or 27 to 47% Ni and not more than 22% Co), 0.005 to 0.1% of Nb, less than 0.01% of C, 0.002 to 0.02% of N, and the balance of Fe and inevitable impurities, wherein the equation "0.000013<=(% Nb)x(% N)<=0.002", is fulfilled. In the alloy, preferably, the maximum grain size of compounds primarily containing Nb and nitrogen and other compounds primarily containing Nb and C is less than 0.5 mum, which can be observed at an fractional section of metal structure, and a total number of the compounds is not less than 50,000/mm2 at an fractional section. An average grain size of the alloy structure is not less than 10 by the crystal grain size number as defined in JIS G0551. The alloy may applied to shadow masks for the Braun tube and lead frames for semiconductor elements.
申请公布号 US2002006350(A1) 申请公布日期 2002.01.17
申请号 US20010810176 申请日期 2001.03.19
申请人 NISHIDA JUNICHI;INOUE RYOJI;SEO TAKEHISA 发明人 NISHIDA JUNICHI;INOUE RYOJI;SEO TAKEHISA
分类号 C21D6/00;C21D6/02;C21D8/02;C22C38/00;C22C38/04;C22C38/08;C22C38/10;C22C38/12;H01J29/07;H01L23/495;(IPC1-7):C22C38/08 主分类号 C21D6/00
代理机构 代理人
主权项
地址