发明名称 Method of joining steel tubes with aluminum ribs
摘要 In a method for joining a steel tube with an aluminum rib, a zinc-aluminum alloy layer, having an aluminum content of 0.5% by wt. to 20% by wt., is applied to the surface of the steel tube or the aluminum rib, and then a fluxing agent in the form of cesium-aluminum tetrafluoride is applied between the steel tube and the aluminum rib at room temperature before or during the mechanical contact of the aluminum rib with the steel tube. The steel tube provided with the aluminum rib is then heated to a soldering temperature of between 370° C. and 470° C. and subjected to room temperature to cool down.
申请公布号 US6715667(B2) 申请公布日期 2004.04.06
申请号 US20020201582 申请日期 2002.07.22
申请人 GEA ENERGIETECHNIK GMBH 发明人 KORISCHEM BENEDICT;DINULESCU HORIA;WITTE RAIMUND;VOLKMER ECKARD
分类号 F16L53/00;B21C37/22;B23K1/00;B23K1/19;B23K35/28;B23K35/363;B23K101/14;B23K103/20;C22C18/04;F16L13/08;F28F1/36;(IPC1-7):B23K31/02;B23K1/20;B23K35/34 主分类号 F16L53/00