发明名称 PROCESS FOR THE PRODUCTION OF POLYMERS OF ACRYLONITRILE AND STYRENE AND OF ACRYLONITRILE STYRENE AND BUTADIENE
摘要 1418228 Coagulating styrene polymer latexes SOC ITALIANA RESINE SIR SpA 18 Dec 1973 [22 Dec 1972] 58656/73 Headings C3P and C3G Latexes of copolymers of styrene, acrylonitrile and optionally butadiene are coagulated in a two stage process by maintaining the latex in a first coagulation stage in the presence of a coagulant at a temperature equal to or up to 15‹ C. higher than the distortion temperature of the polymer (as defined by ASTM standard D 648-56 at 264 p.s.i., carried out on injection moulded specimens of dimensions 5 Î ¢ Î “ inch and conditioned for 24 hours at 50‹ C.) for 10- 100 minutes, and bringing the product thereby obtained to boiling or near boiling conditions in a second coagulation phase carried out in at least two stages, the product being maintained in such conditions for 10-100 minutes in each individual stage. The temperature in the second stage is preferably 98-100‹ C. In the examples: (1) and (3), styrene acrylonitrile copolymer latex is coagulated with CaCl 2 ; and (6) and (9); a graft polymer latex of acrylonitrile and styrene on polybutadiene, is also coagulated with CaCl 2 .
申请公布号 GB1418228(A) 申请公布日期 1975.12.17
申请号 GB19730058656 申请日期 1973.12.18
申请人 SOC ITALIANA RESINE SIR SPA 发明人
分类号 C08F2/00;C08F2/22;C08F6/22;C08F212/00;C08F212/10;C08J3/16;(IPC1-7):C08F6/22 主分类号 C08F2/00
代理机构 代理人
主权项
地址