发明名称 Abrasion and corrosion resistant alloys
摘要 The present invention is directed to air-meltable, tough alloys that are especially resistant to the abrasion and corrosion of wet-process phosphoric acid reactor fluids or slurries, especially those having a high fluoride ion concentration. The instant alloys consist of, by weight, about 22% to about 35% nickel, about 29% to about 35% chromium, about 2% to about 6% molybdenum, about 1% to about 4% copper, about 0.4% to about 1.2% carbon up to about 1.5% each of manganese and silicon and the balance essentially iron plus the usual minor impurities.
申请公布号 US5389334(A) 申请公布日期 1995.02.14
申请号 US19930051633 申请日期 1993.04.22
申请人 CULLING, JOHN H. 发明人 CULLING, JOHN H.
分类号 C22C30/00;(IPC1-7):C22C30/00 主分类号 C22C30/00
代理机构 代理人
主权项
地址