Acrylate elastomers having an improved retention of abrasion resistance after oil immersion, which are readily vulcanized, are prepared with 9 to 59 percent by weight alkoxy alkyl acrylate, 40 to 90 percent by weight alkyl acrylate and about 0.5 to 5.5 percent by weight substituted norbornene compounds. |