ALUMINUM ALLOY SHEET FOR NEGATIVE-PRESSURE CAN LIDS |
摘要 |
This aluminum alloy sheet contains specific amounts of Si, Fe, Mn, and Mg, the balance being Al and unavoidable impurities. The sheet has a recrystallization ratio after hot rolling of not less than 90%. When the texture of a widthwise center portion and widthwise end portions is measured in a cross section taken parallel to the rolling direction at a depth of 1/4 of the thickness from the surface of the sheet, the difference between the area percentage of the cube orientation of the center portion and the area percentage of the cube orientation of the end portions is not more than 10%. The aspect ratio of crystal grains in the surface of the sheet after cold rolling is not less than 5. |
申请公布号 |
WO2016140054(A1) |
申请公布日期 |
2016.09.09 |
申请号 |
WO2016JP54429 |
申请日期 |
2016.02.16 |
申请人 |
KABUSHIKI KAISHA KOBE SEIKO SHO (KOBE STEEL, LTD.) |
发明人 |
TABUCHI Yoshiaki;YAMAGUCHI Masahiro |
分类号 |
C22C21/06;B21B3/00;B65D17/32;C22F1/00;C22F1/047 |
主分类号 |
C22C21/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|