发明名称 ハニカム形状セラミック製分離膜構造体
摘要 The present invention aims to provide a honeycomb-shaped ceramic porous body where the strength reduction upon forming a separation layer is less than conventional porous bodies. The ceramic porous body (9) is provided with a honeycomb-shaped base material (30) and an intermediate layer. At least a part of the ceramic porous body (9) has a structure where aggregate particles are bonded to one another by an inorganic bonding material component. In the ceramic porous body (9), the intermediate layer thickness, which is the thickness of the intermediate layer, is 100 µm or more and 500 µm or less, the base material thickness at the shortest portion between the cells, but excluding the intermediate layer and the separation layer is 0.51 mm or more and 1.55 mm or less, and the ratio of the base material thickness to the intermediate layer thickness is 2.5 or more.
申请公布号 JP6043279(B2) 申请公布日期 2016.12.14
申请号 JP20130505951 申请日期 2012.03.16
申请人 日本碍子株式会社 发明人 寺西 慎;宮原 誠;市川 真紀子;鈴木 秀之
分类号 B01D71/02;B01D69/04;B01D69/10;B01D69/12;B01J35/04;C04B41/85;C04B41/89 主分类号 B01D71/02
代理机构 代理人
主权项
地址