摘要 |
PROBLEM TO BE SOLVED: To provide a laminate film having a polyester melamine resin-based coating layer and a novel structure having smaller &Dgr;haze at 150°C for 1 hour.SOLUTION: There is provided a laminate film having a coating layer on at least a single-side of a polyester film and the coating layer contains a polyester melamine resin of 50 mass% or more based on the mass of the coating layer, the thickness of the coating layer is 100 nm to 5 μm, and a haze variation &Dgr;Hz before and after heat treatment of the laminate film at 150°C for 60 minutes is 1.0% or less. |