发明名称 |
Toner for image formation, and developer and image forming apparatus using the toner |
摘要 |
A toner is provided. The toner includes a crosslinked polyester resin, and a block copolymer. The crosslinked polyester resin includes a diol component, which includes an aliphatic diol component having 3 to 10 carbon atoms in an amount of 50% by mole, and a crosslinked component, which is at least one of a crosslinked component of an aliphatic alcohol having three or more valences and a crosslinked component of an aliphatic acid having three or more valences, and the block copolymer includes a crystalline segment (a) and a non-crystalline segment (b). The toner has a first glass transition temperature (Tg1st) of from 20° C. to 50° C., which is determined by subjecting the toner to differential scanning calorimetry (DSC) and measuring a glass transition temperature in a first temperature rising process in the differential scanning calorimetry (DSC). |
申请公布号 |
US9594322(B2) |
申请公布日期 |
2017.03.14 |
申请号 |
US201414471024 |
申请日期 |
2014.08.28 |
申请人 |
Ricoh Company, Ltd. |
发明人 |
Amemori Suzuka;Sugimoto Tsuyoshi;Saito Akinori;Sawada Toyoshi;Makabe Keiji |
分类号 |
G03G9/087;G03G9/08 |
主分类号 |
G03G9/087 |
代理机构 |
Oblon, McClelland, Maier & Neustadt, L.L.P. |
代理人 |
Oblon, McClelland, Maier & Neustadt, L.L.P. |
主权项 |
1. A toner, comprising:
a crosslinked polyester resin; comprising
a diol component comprising an aliphatic diol component having 3 to 10 carbon atoms in an amount of not less than 50% by mole, anda crosslinked component, which is at least one of a crosslinked component of an aliphatic alcohol having three or more valences and a crosslinked component of an aliphatic acid having three or more valences; a block copolymer comprising
a crystalline polyester segment (a) anda non-crystalline polyester segment (b); and a crystalline polyester resin comprising
a diol component comprising a linear aliphatic diol component having 2 to 12 carbon atoms, anda dicarboxylic acid component comprising a linear aliphatic dicarboxylic having 4 to 12 carbon atoms, wherein the toner has a first glass transition temperature (Tg1st) of from 20° C. to 42° C., wherein the first glass transition temperature (Tg1st) is determined by subjecting the toner to differential scanning calorimetry (DSC) and measuring a glass transition temperature in a first temperature rising process in the differential scanning calorimetry (DSC). |
地址 |