发明名称 |
Elastic terpolymer including diene group and preparation method thereof |
摘要 |
The present invention relates to an elastic terpolymer which can satisfy excellent processability and elasticity (flexibility) at the same time, and a preparation method thereof. The elastic terpolymer is a copolymer of 40 to 70 weight % of ethylene, 15 to 55 weight % of a C3-C20 alpha-olefin, and 0.5 to 20 weight % of a diene obtained in the presence of a group 4 transition metal catalyst, of which i) the weight average molecular weight measured by GPC is 100,000 to 500,000, and ii) Δ tan δ, the difference between the tan δ values at the angular frequencies of 0.2 rad/s and 100.0 rad/s, is 0.5 or less that is measured at 100° C. by using a rubber process analyzer. |
申请公布号 |
US9637579(B2) |
申请公布日期 |
2017.05.02 |
申请号 |
US201314442382 |
申请日期 |
2013.10.14 |
申请人 |
LG Chem, Ltd. |
发明人 |
Yoon Sung-Cheol;Park Sung-Ho;Ko Jun-Seok;Choi Soo-Young |
分类号 |
C08F210/18;C08F236/20;C08F4/653;C08F4/6592;C08L23/16;C08F4/659 |
主分类号 |
C08F210/18 |
代理机构 |
Dentons US LLP |
代理人 |
Dentons US LLP |
主权项 |
1. An elastic terpolymer of 40 to 70 weight % of ethylene, 15 to 55 weight % of a C3-C20 alpha-olefin, and 0.5 to 20 weight % of a diene obtained in the presence of a group 4 transition metal catalyst, of which
i) the weight average molecular weight measured by GPC is 100,000 to 500,000, and ii) Δ tan δ, the difference between the tan δ values at the angular frequencies of 0.2 rad/s and 100.0 rad/s measured at 100° C. by using a rubber process analyzer, is 0.5 or less. |