主权项 |
1. A method for repairing a teak boat deck, built on a leveling surface or an as-built surface, said teak boat deck having a repair area that includes at least one void between teak planks of the teak boat deck and the leveling or as-built surface under the teak boat deck, said method comprising the steps of:
A. inspecting the boat deck for damage and the presence of said at least one void, B. determining the presence of water in said at least one void, C. providing boat deck repair components comprising:
1) a vacuum cover system for providing a vacuum region over the repair area, said vacuum cover system comprising:
a) one or more vacuum blankets for covering the repair area,b) vacuum film covering the vacuum blanket, andc) tape for taping the vacuum film to the boat deck,2) a vacuum suction line for insertion into the vacuum cover system,3) a vacuum pump connected to said vacuum suction line for providing vacuum suction at the repair area,4) a resin supply for line for insertion into the vacuum cover system,5) a resin supply source connected to the resin supply line, D. taping the vacuum film to the boat deck and utilizing vacuum suction the vacuum cover system, the vacuum suction line and the vacuum pump to remove water from the at least one void in the repair area, E. utilizing a heat tunnel, a heat blanket, a heated tent or other heat source to remove moisture from the repair area, F. isolating the repair area by filling perimeter seams between the planks with an epoxy resin to produce splines down to the leveling or the as built surface to isolate the repair area to produce a perimeter boundary below the boat deck to prevent undesired travel of resin, G. masking tops of the planks within the repair area with protective tape, H. filling at least some of the seams within the repair area with sacrificial filler, I. covering the repair area with one of the one or more vacuum cover systems, to create a vacuum region bounded by the vacuum film, the perimeter boundary and the leveling or the as built surface, J. inserting the vacuum suction line into the vacuum region, K. connecting a vacuum pump to said vacuum suction line to provide vacuum in the vacuum region, L. inserting a resin supply line into the vacuum region, M. connecting a resin supply source to said resin supply line, N. turning on said vacuum pump to provide a vacuum suction that draws said resin from said resin supply source through said resin supply line and into said repair area so that said at least one void is filled with said resin, and O. after the resin has dried cutting the sacrificial filler away allowing resin located below the sacrificial filler to remain to create a water tight void free bond below the teak planks. |