发明名称 |
Asphalt mixture, process for production of same, and paving method using same |
摘要 |
An asphalt mixture is provided which comprises an aggregate, an asphalt, a lubricative solidification material and an alkaline additive material that are mixed together. The lubricative solidification material contains a palmitic acid at a ratio of 1 to 15 wt %, a stearic acid at a ratio of 0.3 to 10 wt %, an oleic acid at a ratio of 39 to 59 wt %, a linoleic acid at a ratio of 20 to 48 wt %, and a linolenic acid at a ratio of 1 to 15 wt %. |
申请公布号 |
US9617426(B1) |
申请公布日期 |
2017.04.11 |
申请号 |
US201615175764 |
申请日期 |
2016.06.07 |
申请人 |
Maeda Road Construction Co., Ltd. |
发明人 |
Moriyasu Hirochika;Koshi Kentaro;Taniguchi Hiroshi;Hatakeyama Keigo |
分类号 |
C08L95/00;C08K5/09 |
主分类号 |
C08L95/00 |
代理机构 |
Muncy, Geissler, Olds & Lowe, P.C. |
代理人 |
Muncy, Geissler, Olds & Lowe, P.C. |
主权项 |
1. An asphalt mixture comprising an aggregate, an asphalt, a lubricative solidification material and an alkaline additive material that are mixed together,
wherein the lubricative solidification material contains a palmitic acid at a ratio of from 1 to 15 wt %, a stearic acid at a ratio of from 0.3 to 10 wt %, an oleic acid at a ratio of from 39 to 59 wt %, a linoleic acid at a ratio of from 20 to 48 wt %, and a linolenic acid at a ratio of from 5.5 to 15 wt %. |
地址 |
Tokyo JP |