发明名称 |
Artificial polypeptide fiber and method for producing the same |
摘要 |
An artificial polypeptide fiber of the present invention is an artificial fiber containing a polypeptide as a main component, and has a stress of 350 MPa or more and a toughness of 138 MJ/m3 or more. A method for producing an artificial polypeptide fiber of the present invention is a method for producing the artificial polypeptide fiber obtained by spinning a spinning solution (6) containing a polypeptide derived from natural spider silk proteins and performing drawing of at least two stages. The drawing of at least two stages includes a first-stage drawing (3) in wet heat and a second-stage drawing (4) in dry heat. Thereby, the present invention provides high-toughness artificial polypeptide fibers having favorable stress and rupture elongation, and a method for producing the same. |
申请公布号 |
US9617315(B2) |
申请公布日期 |
2017.04.11 |
申请号 |
US201214114636 |
申请日期 |
2012.05.30 |
申请人 |
SPIBER INC. |
发明人 |
Sekiyama Kazuhide;Sekiyama Kaori;Ishikawa Mizuki;Sato Ryota;Murata Shinya |
分类号 |
C07K14/435;D01F4/02;D01F6/68;D01D5/06;D01D5/16 |
主分类号 |
C07K14/435 |
代理机构 |
Hamre, Schumann, Mueller & Larson, P.C. |
代理人 |
Hamre, Schumann, Mueller & Larson, P.C. |
主权项 |
1. A method for producing an artificial polypeptide fiber that is obtained by spinning a spinning solution containing a polypeptide derived from natural spider silk proteins and performing drawing of at least two stages, wherein the drawing of at least two stages includes a first-stage drawing in wet heat and a second-stage drawing in dry heat, and
an ambient temperature at the time of the second-stage drawing is in a range from 170 to 270° C. |
地址 |
Yamagata JP |