发明名称 Method And Apparatus For Producing Milled Elastomer
摘要 The invention is a method for producing milled elastomer, comprising the steps of directing a liquid jet from at least one nozzle on an elastomeric material moving in an at least partially transversal direction with respect to the discharge direction of the at least one nozzle. In the method according to the invention the liquid jet directed on the elastomeric material has a pressure of 650-1350 bar, and the elastomeric material is moved with respect to the at least one nozzle such that, in a first phase adapted for disintegrating a surface of the elastomeric material, the elastomeric material has a first forward-feed rate of 10 to 20 mm/s at a point of impact of the liquid jet in a direction transverse to the discharge direction, and, in a second phase after disintegrating the surface, the elastomeric material has a second forward-feed rate being decreased with 35-65% compared to the first forward-feed rate. The invention is, furthermore, an apparatus for producing milled elastomer.
申请公布号 US2017080604(A1) 申请公布日期 2017.03.23
申请号 US201415310478 申请日期 2014.12.05
申请人 AquaJet Zrt. 发明人 Moldovan Gyorgy;Kostyal Gabor;Kostyal Ferenc Gyorgy;Csako Antal
分类号 B29B17/04;B29B17/02 主分类号 B29B17/04
代理机构 代理人
主权项 1. A method for producing milled elastomer, comprising the steps of directing a liquid jet from at least one nozzle (38) on an elastomeric material moving in an at least partially transversal direction with respect to the discharge direction of the at least one nozzle (38),characterised in that the liquid jet directed on the elastomeric material has a pressure of 650-1350 bar, and the elastomeric material is moved with respect to the at least one nozzle (38) such that, in a first phase adapted for disintegrating a surface of the elastomeric material, the elastomeric material has a first forward-feed rate of 10 to 20 mm/s at a point of impact of the liquid jet in a direction transverse to the discharge direction, and, in a second phase after disintegrating the surface, the elastomeric material has a second forward-feed rate being decreased with 35-65% compared to the first forward-feed rate.
地址 Harta HU