An aluminium-silicon-manganese-iron alloy which comprises (by weight): 8-12 % silicon, up to around 0.30 % iron, manganese in an amount that is greater than the amount of iron present, less than 0.1 % magnesium and the balance being aluminium. The iron : manganese ratio preferably lies in the range 0.2-0.8. The alloy can be used to make die casting products for automotive and aerospace applications, with the products being heat treated at a temperature in the range 350-390 0C.
申请公布号
EP3143174(A1)
申请公布日期
2017.03.22
申请号
EP20150723479
申请日期
2015.05.12
申请人
Jaguar Land Rover Limited
发明人
IKWUEZE, Emeka;BLACKMORE, Pete;BROUGH, Ashley;RUFFLE, Simon;MURCOTT, Wayne