发明名称 酸化物超電導線材及びその製造方法
摘要 PROBLEM TO BE SOLVED: To provide an oxide superconductive wire material preventing deterioration of superconductive property by water immersion from an end.SOLUTION: There is provided an oxide superconductive wire material 1 obtained by laminating an intermediate layer, an oxide superconductive layer and a stabilization layer on a tape-like base material, and a coating member 21 is deposited at both ends in a longer direction 1a of the oxide superconductive wire material 1. The oxide superconductive wire material 1 contains a metal member 40 and a connection layer 42 formed on at least a face opposite with the oxide superconductive wire material 1 of the metal member 40.
申请公布号 JP6101491(B2) 申请公布日期 2017.03.22
申请号 JP20130002175 申请日期 2013.01.09
申请人 株式会社フジクラ 发明人 日高 輝
分类号 H01B12/06;C01G1/00;C01G3/00;H01B12/02;H01B13/00;H01F17/00;H01F27/00;H01F41/00;H01R4/68;H01R43/02 主分类号 H01B12/06