发明名称 INTERNAL MIXTURE FOR A TYRE HAVING IMPROVED CRACKING RESISTANCE
摘要 A tire comprises at least one internal rubber composition having improved cracking resistance, the said internal composition comprising at least 50 to 100 phr of an isoprene elastomer such as natural rubber; optionally, 0 to 50 phr of another diene elastomer such as BR or SBR; 0 to less than 15 phr of a carbon black; between 40 and 100 phr of a nanoscale inorganic filler such as silica. The internal composition is free from or comprises less than 2%, expressed relative to the weight of the nanoscale inorganic filler of (elastomer/inorganic filler) coupling agent.
申请公布号 EP2999741(B1) 申请公布日期 2017.03.22
申请号 EP20140719007 申请日期 2014.04.23
申请人 Compagnie Générale des Etablissements Michelin;MICHELIN Recherche et Technique S.A. 发明人 NAKASHIMA, Yasufumi;PAGANO, Salvatore
分类号 C08K3/36;B60C1/00;C08K3/00;C08L7/00 主分类号 C08K3/36