发明名称 Clay mineral for reducing inorganic phosphates, in particular in renal replacement therapy
摘要 The invention relates to a clay mineral for use as an agent for reducing the concentration of inorganic phosphate in liquids, in particular in bodily fluids or dialysis liquids, in order to treat hyperphosphatemia, in particular in a renal replacement therapy, wherein before use, the clay mineral is thermally treated at a temperature between 400° C. and 800° C., preferably between 500° C. and 700° C., in particular preferably at 550° C., over a time period of 60 min to 240 min, preferably 90 min to 180 min, in particular preferably 120 min.
申请公布号 US9585913(B2) 申请公布日期 2017.03.07
申请号 US201314405734 申请日期 2013.05.31
申请人 Fraunhofer-Gesellschaft zur Förderung der angewandten Furschung e.V. 发明人 Mitzner Steffen;Kerkhoff Claus;Emmrich Frank;Breitruck Anne;Bodammer Peggy;Kruger Gerd;Dallwig Rainer
分类号 A61K33/06;A61K45/06;A61K33/12;A61K35/02;A61K9/00;A61K9/14 主分类号 A61K33/06
代理机构 The Webb Law Firm 代理人 The Webb Law Firm
主权项 1. A silicate clay mineral for use as agent for reducing the concentration of inorganic phosphate in bodily fluids or dialysis fluids for the treatment of hyperphosphatemia, wherein the silicate clay mineral has a mean particle size of 0.1 to 3 μm and is thermally treated before use at a temperature between 400° C. and 800° C. over a period of 60 min to 240 min.