Manufacturing method of poly lactic acid stereocomplex using solvent casting method |
摘要 |
Disclosed is a method for manufacturing a polylactic acid film. More specifically, the present invention relates to a method for stably and effectively obtaining optimized stereocomplex crystals through specified boiling point and evaporation time of a solvent allowing the content of stereocomplex crystals to be 100%. |
申请公布号 |
US9580561(B2) |
申请公布日期 |
2017.02.28 |
申请号 |
US201113286480 |
申请日期 |
2011.11.01 |
申请人 |
Hyundai Motor Company;KOREA UNIVERSITY OF TECHNOLOGY AND EDUCATION INDUSTRY-UNIVERSITY COOPERATION FOUNDATION |
发明人 |
Hong Chae Hwan;Han Do Suck;Nam Byeong Uk |
分类号 |
C08G63/08;C08J3/00;C08J5/18;C08L67/04 |
主分类号 |
C08G63/08 |
代理机构 |
Mintz Levin Cohn Ferris Glovsky and Popeo, P.C. |
代理人 |
Mintz Levin Cohn Ferris Glovsky and Popeo, P.C. ;Corless Peter F. |
主权项 |
1. A method for manufacturing a polylactic acid stereocomplex film, comprising the steps of:
(1) selecting a solvent whose boiling point ranges from 39.6° C. to 130.5° C.; (2) calculating minimum evaporation time required to achieve 100% of stereocomplex crystals by evaporating the selected solvent using Equation 1
y=0.0042x2−0.2769x+10±5 Equation 1 wherein x is the boiling point of the selected solvent, and y is the minimum evaporation time required to achieve 100% of stereocomplex crystals by evaporating the selected solvent in hours; (3) mixing only poly-L-lactic acid and poly-D-lactic acid in a solvent; and (4) evaporating the selected solvent for the minimum evaporation time calculated in step (2) at 20˜30° C., wherein the polylactic acid stereocomplex film consists of 100% of stereocomplex crystals of the poly-L-lactic acid and the poly-D-lactic acid, and the minimum evaporation time calculated in step (2) ranges from 0.6 hour to 50.4 hours. |