发明名称 Resin-soluble thermoplastic veil for composite materials
摘要 A resin-soluble thermoplastic polymer veil toughening element for a curable composition wherein the polymer element is a non-woven veil in solid phase adapted to undergo at least partial phase transition to fluid phase on contact with a component of the curable resin matrix composition in which it is soluble at a temperature which is less than the temperature for substantial onset of gelling and/or curing of the curable composition and which temperature is less than the polymer elements melt temperature; a method for the preparation thereof, a preform support structure for a curable composition comprising the at least one thermoplastic veil element together with structural reinforcement fibers, methods for preparation thereof, a curable composition comprising the at least one thermoplastic veil element or the support structure and a curable resin matrix composition, a method for preparation and curing thereof, and a cured composite or resin body obtained thereby, and known and novel uses thereof.
申请公布号 US9566762(B2) 申请公布日期 2017.02.14
申请号 US201414226928 申请日期 2014.03.27
申请人 Cytec Technology Corp. 发明人 Lo Faro Carmelo;Abusafieh Abdel;Webb William Erwin;Doyle Marc
分类号 B32B5/02;B32B5/26;B32B5/08;B32B7/10;C08J5/04 主分类号 B32B5/02
代理机构 代理人 Dang Thi D.
主权项 1. A thermoplastic toughening element for resin infusion manufacturing of composite comprising: a layer of a plurality of resin-soluble thermoplastic fibers randomly oriented and adhered to one another into a veil consisting of the resin soluble thermoplastic fibers with an areal weight of about 5 to about 80 gsm, wherein the toughening element is interposed between and in direct contact with adjacent plies consisting of structural reinforcement fibers, wherein the resin-soluble thermoplastic fibers are in a solid phase and undergo at least partial phase transition to a fluid phase on contact with a curable resin matrix in which the thermoplastic fibers are soluble at a first temperature for substantial dissolution, which is less than a second temperature for substantial onset of curing of the curable resin matrix, and wherein the concentration of toughening element is highest in the resin matrix between the adjacent plies and decreases in concentration as the matrix approaches the plies.
地址 Wilmington DE US