发明名称 熱間または冷間低密度圧延鋼、この実施方法および使用
摘要 A rolled steel sheet is provided. The rolled steel sheet has a mechanical strength greater than or equal to 600 MPa and an elongation at fracture that is greater than or equal to 20%. A a method for its fabrication is also provided. The chemical composition of the steel sheet includes 0.10≦̸C≦̸0.30%, 6.0≦̸Mn≦̸15.0%, 6.0≦̸Al≦̸15.0%, and optionally one or more elements selected from among: Si≦̸2.0%, Ti≦̸0.2%, V≦̸0.6% and Nb≦̸0.3%. The remainder of the composition includes iron and the unavoidable impurities resulting from processing. The ratio of the weight of manganese to the weight of aluminum is such that Mn Al > 1.0 . The microstructure of the sheet includes ferrite, austenite and up to 5% Kappa precipitates in area fraction.
申请公布号 JP6074031(B2) 申请公布日期 2017.02.01
申请号 JP20150514609 申请日期 2013.05.27
申请人 アルセロルミタル・インベステイガシオン・イ・デサロジヨ・エセ・エレ 发明人 スアソ・ロドリゲス,ラン・アルベルト;ペルラド,アストリッド;ガラ,グザビエ
分类号 C22C38/00;C21D8/02;C21D9/46;C22C38/14 主分类号 C22C38/00