发明名称 電気化学素子正極用複合粒子の製造方法
摘要 PROBLEM TO BE SOLVED: To provide a process of manufacturing a composite particle for a positive electrode of an electrochemical element, excellent in dispersion of a conductive agent even when a water type slurry is used, and having low resistivity when it is made to be a battery.SOLUTION: The process of manufacturing a composite particle for a positive electrode of an electrochemical element includes the steps of: obtaining a slurry by dispersing a positive electrode active material, a conductive agent, and a binder into water; and obtaining a granulation particle by spray drying and granulating the slurry, wherein a ratio of degree of hydrophobicity (a positive electrode active material/a conductive agent) of the positive electrode active material and the conductive agent obtained by a methanol method is 0.5 or more and 1.5 or less.
申请公布号 JP6070243(B2) 申请公布日期 2017.02.01
申请号 JP20130026527 申请日期 2013.02.14
申请人 日本ゼオン株式会社 发明人 松村 卓
分类号 H01M4/525;H01M4/36;H01M4/505 主分类号 H01M4/525