发明名称 |
METHOD FOR IMPROVING THE STRUCTURE OF A STEEL COMPONENT AFTER HEATING AND STELL COMPONENT OBTAINED BY THE METHOD |
摘要 |
The present disclosure relates to a method for improving the steel structure of a steel component after heating including the steps of heating the steel component to a temperature of at least 1100° C., quenching the steel component to a temperature above the martensite start temperature (Ms) to form bainite, and maintaining the steel component at that temperature for a holding time sufficient for transformation of all austenite to bainite, re-heating the steel component to a temperature of at least 580° C. but below the Ac1 transformation temperature, and maintaining the steel component at that temperature for the steel component to exhibit a hardness of 45 Rockwell hardness C or below, and cooling the steel component. |
申请公布号 |
US2016348204(A1) |
申请公布日期 |
2016.12.01 |
申请号 |
US201615163636 |
申请日期 |
2016.05.24 |
申请人 |
Aktiebolaget SKF |
发明人 |
Larsson Staffan |
分类号 |
C21D9/40;C21D6/00;C21D1/25;F16C33/62;F16C33/64 |
主分类号 |
C21D9/40 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method for restoring a steel structure for a steel component after heating characterized in that it comprises the steps of:
a) heating a steel component to a temperature of at least 1100° C., b) quenching the steel component to a temperature above the martensite start temperature (Ms) to form bainite, and maintaining the steel component at that temperature for a holding time sufficient for transformation of all austenite to bainite, c) re-heating the steel ring to a temperature of at least 580° C. but below the Ac1 transformation temperature, and maintaining the steel ring at that temperature for the steel ring to exhibit a hardness of 45 Rockwell hardness C or below, d) cooling the steel ring. |
地址 |
Goteborg SE |