METHOD FOR PREPARING NAY MOLECULAR SIEVE OF HIGH SILICA-ALUMINA RATIO AND PRODUCT THEREOF |
摘要 |
The present invention relates to a method for preparing a NaY molecular sieve having a high silica-to-alumina ratio, wherein deionized water, a silicon source, an aluminum source, an alkali source, and ILs as a template agent are mixed to obtain an initial gel mixture; the initial gel mixture is maintained at a proper temperature and aged, then fed into a high pressure synthesis kettle for crystallization; the solid product is separated and dried, to obtain the NaY molecular sieve having a high silica-to-alumina ratio, wherein the ILs is a short-chain alkylimidazolium ionic liquid. The template agent used in the method of the invention is less volatile, and the resultant high-silicon Y molecular sieve has a high crystallinity and a silica-to-alumina ratio of 6 or more. |
申请公布号 |
EP3081532(A1) |
申请公布日期 |
2016.10.19 |
申请号 |
EP20130899055 |
申请日期 |
2013.12.09 |
申请人 |
DALIAN INSTITUTE OF CHEMICAL PHYSICS, CHINESE ACADEMY OF SCIENCES |
发明人 |
YUAN, DANHUA;DONG, XINGLONG;XU, YUNPENG;LIU, ZHONGMIN;WANG, KUNYUAN;HUANG, WEI |
分类号 |
C01B39/24 |
主分类号 |
C01B39/24 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|