发明名称 Lower cost high strength single crystal superalloys with reduced Re and Ru content
摘要 A first embodiment of a nickel based alloy consists essentially of from 3.0 to 5.2 wt% chromium, from 1.5 to 3.0 wt% molybdenum, from 6.0 to 12.5 wt% tungsten, from 5.0 to 11 wt% tantalum, from 5.5 to 6.5 wt% aluminum, from 11 to 14 wt% cobalt, from 0.001 to 1.75 wt% rhenium, from 0.2 to 0.6 wt% hafnium, up to 0.05 wt% yttrium, up to 3.0 wt% ruthenium, and the balance nickel. Another embodiment of a nickel based alloy consists essentially of from 1.0 to 3.0 wt% chromium, up to 2.5 wt% molybdenum, from 11 to 16 wt% tungsten, from 4.0 to 8.0 tantalum, from 5.7 to 6.5 wt% aluminum, from 11 to 15 wt% cobalt, from 2.0 to 4.0 wt% rhenium, from 0.2 to 0.6 wt% hafnium, up to 0.05 wt% yttrium, up to 3.0 wt% ruthenium, and the balance nickel.
申请公布号 EP2218798(B1) 申请公布日期 2016.09.14
申请号 EP20090252708 申请日期 2009.12.01
申请人 UNITED TECHNOLOGIES CORPORATION 发明人 CETEL, ALAN D.;SHAH, DILIP M.
分类号 C22C19/05 主分类号 C22C19/05
代理机构 代理人
主权项
地址