摘要 |
There is provided a multilayer film comprising a layer (X) containing a polyvinyl acetal (I) having an acetalization degree of 55 to 80 mol%, a content of a vinyl ester monomer unit of 0.1 to 1.5 mol% and a viscosity-average degree of polymerization of 1,400 to 5,000; and a layer (Y) containing a polyvinyl acetal (II) having an acetalization degree of 70 to 85 mol%, a content of a vinyl ester monomer unit of 5 to 15 mol% and a viscosity-average degree of polymerization of 1,400 to 5,000, wherein the multilayer film satisfies formulas (1) and (2): (A-B)/A < 0.80 (1) and 1.00 × 10 -2 < (b/y)/(a/x) < 2.00 × 10 -1 (2). There is thus provided a film which exhibits sufficient sound-absorbability, resistance to coloration by heating, reduction in foreign materials (undissolved materials) and excellent recyclability. |