摘要 PROBLEM TO BE SOLVED: To provide a welding method and a welding structure that hardly cause cracks due to creep damage in a weld heat affected zone by long time use even if a main steam temperature exceeds 560°C and facilitate control of welding and heat treatment.SOLUTION: A welding method includes the steps of: laminating a welding metal layer 10 of a predetermined build-up height using a Ni-based alloy welding material at the position for attaching a heat transfer tube, on an outer diameter surface of a header 1 comprising a ferrite-based steel; working a tube hole 1a substantially in the center of the welding metal layer 10; forming one side of a groove on a height-direction end surface of the welding metal layer 10; and welding the heat transfer tube 4 to the header 1 by butt welding, the heat transfer tube 4 having the other side of butt groove formed on the end surface and comprising an austenitic stainless steel or Ni-based alloy, to the header 1 . Also, a welded structure is obtained by the method.
申请公布号 JP5979665(B2) 申请公布日期 2016.08.24
申请号 JP20120179411 申请日期 2012.08.13
申请人 三菱日立パワーシステムズ株式会社 发明人 原田 英政;菊原 誠治;重森 久典
分类号 B23K9/028;B23K9/00;B23K9/04;B23K9/167;B23K33/00;F22B37/22 主分类号 B23K9/028
代理机构 代理人
主权项
地址