摘要 |
First, a first porous body is manufactured by stretching, in a uniaxial direction, a sheet made of polytetrafluoroethylene having a standard specific gravity of 2.155 or more, and a second porous body is manufactured by stretching, in biaxial directions, a sheet made of polytetrafluoroethylene. Next, the first porous body is integrated with the second porous body by stretching a laminate of the first porous body and the second porous body in the same direction as the uniaxial direction while heating the laminate at a temperature equal to or higher than a melting point of polytetrafluoroethylene. Thus, a porous polytetrafluoroethylene membrane is produced. |