发明名称 精製多糖類繊維の製造方法、ゴム−繊維複合体の製造方法、補強用コードの製造方法、ゴム−コード複合体の製造方法、及びタイヤの製造方法
摘要 PROBLEM TO BE SOLVED: To provide a purified polysaccharide fiber manufactured by using a raw material with less environmental load due to suppression of carbon disulfide emission, where the purified polysaccharide fiber can impart excellent performances in terms of steering stability, riding quality and durability when used for a tire; a rubber-fiber composite; a cord for reinforcing; a rubber-cord composite; and a tire excellent in tire properties, using the same.SOLUTION: The purified polysaccharide fiber of the present invention is characterized in that the relation of strength TB(cN/dtex) and breaking elongation EB(%) at 25°C satisfies the formulas (1) and (2) and also the relation of elastic modulus Er(%) and breaking elongation EB(%) at 25°C satisfies the formula (3) and that the percentage ([Eh/Er] x 100) of elastic modulus Eh(%) to the Er(%) at 150°C is 75 to 100(%).
申请公布号 JP5948144(B2) 申请公布日期 2016.07.06
申请号 JP20120116083 申请日期 2012.05.21
申请人 株式会社ブリヂストン 发明人 小出 光治
分类号 D01F2/00;B60C9/00;D02G3/48 主分类号 D01F2/00
代理机构 代理人
主权项
地址